FIELD metallurgy. SUBSTANCE method includes antimony and lead leaching from copper anode slime in a solution containing 50-200 g/dm 3 of glycerin, 50-100 g/dm 3 of alkali and a reducing agent, in an amount that provides the system oxidation-reduction potential more positively than 0.8 V at a temperature of 70-90 C for 2-3 hours. Thus lead from the leach solution is educed by known methods.